Conventional HSS

Standards

  • Europe : HS 18-0-1
  • Sweden : SS2750
  • Japan : JIS SKKH2
  • Germany : 1.3355
  • USA : AISI T1

Delivered Hardness

  • Soft annealed : 260 HB
  • Cold drawn : 285 HB
  • Cold rolled : 285 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Conventional HSS

Standards

  • Europe : HS 2-9-1-8
  • Sweden : SS2723
  • Japan : JIS SKH59
  • Germany : 1.3247
  • USA : AISI M42

Delivered Hardness

  • Soft annealed : 270 HB
  • Cold drawn : 295 HB
  • Cold rolled : 295 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Conventional HSS

Standards

  • Europe : HS 6-5-2-5
  • Sweden : SS2723
  • Japan : JIS SKH55
  • Germany : 1.3243
  • USA : AISI M35

Delivered Hardness

  • Soft annealed : 260 HB
  • Cold drawn : 285 HB
  • Cold rolled : 285 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Conventional HSS

Standards

  • Europe : HS 6-5-2
  • Sweden : SS 2722
  • Japan : JIS SKH51
  • Germany : 1.3343
  • USA : AISI M2

Delivered Hardness

  • Soft annealed : 250 HB
  • Cold drawn : 275 HB
  • Cold rolled : 275 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Conventional HSS

Standards

  • Europe : HS 2-9-1
  • Germany : 1.3346
  • USA : AISI M1

Delivered Hardness

  • Soft annealed : 250 HB
  • Cold drawn : 275 HB
  • Cold rolled : 275 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Powder metallurgy HSS

Standards

  • Europe : HS 4-3-8
  • Germany : 1.3352

Delivered Hardness

  • Soft annealed : 300 HB
  • Cold drawn : 325 HB
  • Cold rolled : 325 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Powder metallurgy HSS

Standards

  • Europe : HS 6-5-3-8
  • Sweden : SS 2726
  • Germany : 1.3294

Delivered Hardness

  • Soft annealed : 290 HB
  • Cold drawn : 315 HB
  • Cold rolled : 315 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Powder metallurgy HSS

Standards

  • Europe : HS 6-5-3C
  • Sweden : SS 2725
  • Japan : JIS SKH53
  • Germany : 1.3395
  • USA : AISI M3:2

Delivered Hardness

  • Soft annealed : 260 HB
  • Cold drawn : 285 HB
  • Cold rolled : 285 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms