Chemical composition

C Si Mn Cr Mo W V
0.60 1.0 0.3 4.0 2.0 2.1 1.5

Standards

  • Europe : HS 2-2-2
  • Germany : 1.3397

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Heat treatment

Delivered Hardness

  • Soft annealed : 230 HB

Characteristics

ASP®2012 can be worked as follows:

  • machining (grinding, turning, milling)
  • polishing
  • hot forming
  • electrical discharge machining
  • welding (special procedure including preheating and filler materials of base material composition).